Examples

Drill pipes

Application, field
Material
Bonding dimensions

φ130.2×t18

Conventional technique

Merits of Adopting Izumi Equipment

Conventional technology: flash butt welding

Issues to be resolved

Flash butt welding
- Low bonding strength, use not possible for long parts
- Excavation depth limit of 2,000 m

Adoption merits

- Improved bonding strength with pressure welding
- Excavation possible to depth of 12,000 m

Applicable Model

Examples of Other Fields / Merits

Woodworking drills (gimlets)
Woodworking drills (gimlets)

SS400×S55C

Brake torque plates
Brake torque plates

S35C×S35C

Torsion bars
Torsion bars

S45C×SUP435

Pipe supports
Pipe supports

SS41×STKM38×STKM38

Click here for list of examples

Friction welding materials

Stable, complete joints are realized, even when combining dissimilar metals or nonferrous metals.

Inquiries