Examples

Branch joints

Application, field
Material
Bonding dimensions

φ47×t1

Conventional technique

Merits of Adopting Izumi Equipment

Conventional technology: forged part cutting

Issues to be resolved

Cutting from integrated forged parts
- High machining workload
- High material cost

Adoption merits

- Screw and body bonding by machining workpieces separately
- Welding after threading
- Reduced machining workload
- Reduced blank cost

Applicable Model

Examples of Other Fields / Merits

Counter gears
Counter gears

S43C×S43C

Tulip shafts
Tulip shafts

SCr421×SCM435

Back rollers
Back rollers

S45C×SS400×STKM38

Spools
Spools

Aluminum x electromagnetic steel

Click here for list of examples

Friction welding materials

Stable, complete joints are realized, even when combining dissimilar metals or nonferrous metals.

Inquiries